Yes, your main concern should be redissolution and adhesion; Epoxy paint is two-component, after curing, the solvent of alkyd blending paint can not dissolve epoxy paint, and there is no possibility of redissolving, if the blending paint is brushed with epoxy paint, your worries are necessary, as long as the surface cleanliness is enough, there is no problem with adhesion, but epoxy paint is best to use brush and roller coating, so that the surface of the paint film can form a frosted surface, and it can improve the adhesion of the blending paint (the surface finish of spraying is too high but not good).
-
OK. In general, epoxy paints are used for indoor (due to the poor weather resistance of epoxy resins) heavy corrosion protection. Please consider the pH level around the painted object, and if you need heavy anti-corrosion, please use a matching topcoat, as alkyd paints are absolutely unacceptable.
Epoxy micaceous iron antirust paint is a two-component antirust paint composed of epoxy resin, mica iron oxide, additives, solvents, etc. The paint film is tough and has excellent adhesion. Water resistance, water vapor permeation resistance, good sealing, oil resistance, solvent resistance and chemical resistance.
-
If the alkyd blended lacquer coating for a long time is not too much of a problem, the new painting, fluorocarbon bite-alkyd primer.
-
Can not be used like this, alkyd paint can only be used in alkyd paint, can not use other paint, with epoxy micaceous iron intermediate paint will bite the bottom, paint film peeling off, epoxy micaceous iron intermediate paint can be used with epoxy primer.
-
Polishing it out, there will be problems.
-
No, what are you using to make the first round search primer, if you use the second base of the cloud iron which high between the paint, then you use the blending paint as the topcoat will not react, it is a bit of a luxury, you can use the alkyd bottom! Also, may I ask which Li Ruler region are you???
-
You can brush the blending paint without problems, the primer must be dry to the end.
The general matching will not be used in this way, and the epoxy sealing primer is also a two-component topcoat, such as polyurethane paint, acrylic polyurethane topcoat, etc., and the alkyd blending paint can be said to be a high-grade primer, with a low-end topcoat, which is not very suitable.
-
Is the alkyd blended paint underneath? If so, there is a risk of biting the bottom of the epoxy micaceous iron intermediate paint on the back. The surface should be painted with one-component paints, such as alkyd, chlorinated rubber, chloroether, chlorosulfonated polyethylene, etc. Alkyd blended paint is not weather-resistant. Wu Han Hurst, Yang.
It is recommended to cover the coat with an acrylic topcoat for the finish.
-
Epoxy micaceous iron antirust paint is used as a primer, and epoxy micaceous iron intermediate paint is used in combination with primer and topcoat.
-
Yes, the adhesion of epoxy micaceous iron intermediate paint is also very good, and there is no problem with using it directly as a primer, but if there is a primer, it is recommended to apply the primer first, after all, the adhesion of epoxy zinc-rich primer is much better than that of epoxy micaceous iron intermediate paint.
Epoxy micaceous iron antirust paint (intermediate paint) composition: antirust paint composed of epoxy resin, mica iron oxide, plasticizer, additives and solvents.
Main characteristics: The permeability of water vapor and oxygen varnish film is low, and it has excellent water resistance and good corrosion resistance.
It dries quickly, several times faster than that of oil-based paints.
It has excellent low-temperature construction performance and can be applied in -20 50 environments.
The paint film has good adhesion to steel
The paint film layer is intermiscible with each other, and has excellent interlayer adhesion. Old paint in chlorinated rubber.
When the film is repaired and painted again, it is not necessary to remove the firm old paint film, which is convenient for maintenance.
The paint film is not saponifiable in seawater, and has a good matching performance with cathodic protection.
It has good durability.
It is suitable for anti-rust at the bottom of the ship, the waterline of the ship, the anti-corrosion of the offshore steel structure building and other steel structures, and can also be used as a protective layer for concrete engineering facilities.
I am a professional manufacturer of industrial anticorrosive paint, you can contact me if you have any needs.
-
Epoxy micaceous iron intermediate paint can be used as a primer in individual cases, or when the anti-corrosion requirements are not strict, but it is usually not recommended to be used as a primer, and it is also possible to use ordinary epoxy primer.
The previous supporting scheme is epoxy zinc-rich primer + epoxy micaceous iron intermediate paint + anti-corrosion topcoat, if you want to save a layer of paint, it is recommended to remove the intermediate paint link, and use epoxy zinc-rich primer + anti-corrosion topcoat, the anti-corrosion effect will be much better than the intermediate paint primer.
If you consider the cost of paint, you can choose the scheme of epoxy anticorrosive primer + anticorrosive topcoat, the price of epoxy anticorrosive primer is lower than that of zinc-rich primer, and the anti-corrosion effect is also very good.
-
The shielding ability of epoxy micaceous iron is good, but the adhesion is average, and the anti-rust ability is not good, so it is recommended not to save the primer.
-
Whether epoxy intermediate paint can be used as a primer depends on the actual working conditions.
Epoxy micaceous iron intermediate paint (primer) is composed of gray mica iron oxide as pigment, epoxy resin as the base material, and polyamide resin as the curing agent. Due to the superior properties of mica iron oxide and epoxy resin, the paint film is tough, with good adhesion, flexibility, wear resistance and sealing properties.
It can be used as the middle layer of high-performance anti-rust primer, such as epoxy iron red primer, epoxy zinc-rich primer, and inorganic zinc primer, to protect the primer paint film and enhance the protective performance of the entire coating.
-
The general construction step is to brush the alkyd antirust paint first, and after drying for 24 hours, brush the alkyd blending paint, which is a more correct and reasonable construction method. However, it should be noted that the two paints cannot be mixed together, and the characteristics of the raw materials are different. There is also a 24-hour coating interval, otherwise it is easy to bite the bottom and blister.
-
The epoxy cloud iron is one of the most important paint varieties after alkyd phenolic iron, and is widely used in heavy anticorrosive coating systems as anti-rust base paint and intermediate paint. Epoxy micaceous iron anti-rust paint, as the name suggests, was first used as an anti-rust base paint.
How about epoxy grinding stone flooring? Epoxy grinding stone flooring**? >>>More
1. The concrete strength must be C25Contains more than 350kg of m3 of common silicate. cement and water-cement ratio <; 2. The screed must be fine stone concrete and its thickness shall not be less than 50 mm. >>>More
Specifically, you can consult Beijing Katuo Construction Engineering, Beijing Katuo Construction Engineering's business is widely distributed in residential, automobile manufacturing, machinery, chemical, electronics, medicine, tobacco, papermaking, education, printing, food, supermarkets and other industries, and constantly provide perfect system solutions for these industries to meet individual needs. Looking forward to hearing from you!
Steps to brush epoxy floor paint:
1.Clean the floor: Start by cleaning the floor and removing all dust, oil, and debris. >>>More
There are three main differences between painted epoxy flooring and self-leveling epoxy flooring: >>>More