Can tempered glass open holes? Can tempered glass be punched

Updated on home 2024-02-09
25 answers
  1. Anonymous users2024-02-06

    No holes can be opened.

    Only before tempering, the holes are machined and then tempered. If you want to open the hole, you need to open it before the glass is tempered, and then tempered. Temperedglass reinforcedglass belongs to safety glass.

    Tempered glass is actually a kind of prestressed glass, in order to improve the strength of the glass, chemical or physical methods are usually used; Compressive stress is formed on the surface of the glass, and the surface stress is first offset when the glass is subjected to external force, so as to improve the bearing capacity and enhance the wind pressure resistance, cold and heat resistance, impact and so on. Note the difference with FRP.

  2. Anonymous users2024-02-05

    Toughened glass. I can't open the hole anymore. Only before tempering, the holes are machined and then tempered. If you want to open the hole, you need to open it before the glass is tempered, and then tempered.

  3. Anonymous users2024-02-04

    Tempered glass should never be opened. Tempered glass is actually a kind of prestressed glass, in order to improve the strength of the glass, chemical or physical methods are usually used to form compressive stress on the surface of the glass, and the surface stress is first offset when the glass bears external force, so as to improve the bearing capacity and enhance the wind pressure resistance, cold and heat resistance, impact and so on; The strength of tempered glass is several times higher than that of ordinary glass, the flexural strength is 3 5 times that of ordinary glass, and the impact strength is 5 10 times that of ordinary glass. Its increased bearing capacity improves its fragile properties, and even if the tempered glass is broken, it is a small fragment without acute angles, and the damage to the human body is greatly reduced.

    The resistance of tempered glass to quenching and heating is 2 to 3 times higher than that of ordinary glass, and it can generally withstand more than 150 temperature changes, which has obvious effects on preventing thermal explosion.

    Therefore, the tempered glass can no longer be cut and processed, and the glass can only be processed to the required shape before tempering, and then tempered.

  4. Anonymous users2024-02-03

    Tempered glass cannot be opened. Before the tempering process, the hole should be opened, and then it should be fired at a high temperature, that is, tempered.

    If you take tempered glass to open the hole, the result is to burst.

  5. Anonymous users2024-02-02

    It didn't work before, and it didn't work under general conditions, and the special laser equipment can be opened, but I've only heard of it, and I haven't seen it.

  6. Anonymous users2024-02-01

    OK. But with professional tools! It's dangerous to make it yourself!

  7. Anonymous users2024-01-31

    Tempered glass that is not thick can be corroded with hydrofluoric acid to create holes.

  8. Anonymous users2024-01-30

    No, the tempered glass should be drilled and ground before tempering.

  9. Anonymous users2024-01-29

    Tempered glass cannot be perforated. Because the compressive stress of the glass surface is adjusted in the production process of tempered glass, once the tempered glass is punched, the tempered glass will be broken into honeycomb obtuse small particles because the balance of uniform compressive stress is destroyed, and it will no longer be used, so it is not allowed to punch holes for tempered glass.

    Tempered Glass Introduction:Temperedglass reinforcedglass belongs to safety glass. Tempered glass is actually a kind of prestressed glass, in order to improve the strength of the glass, chemical or physical methods are usually used to form compressive stress on the surface of the glass, and the surface stress is first offset when the glass bears external force, so as to improve the bearing capacity and enhance the wind pressure resistance, cold and heat resistance, impact and so on;

    Note the difference with FRP.

  10. Anonymous users2024-01-28

    Professional personnel can, but they must not do it privately. It must be carried out by professional personnel so as not to cause damage to the tempered glass.

    Tempered glass belongs to safety glass, that is, in its strengthening process has been adjusted to the compressive stress of the glass surface to the state, so when the tempered glass is treated, it is strictly forbidden to do any cutting or punching, once this is done, then the glass will be broken into honeycomb obtuse small particles because the balance of uniform compressive stress is destroyed.

  11. Anonymous users2024-01-27

    OK. Rules for tempered glass openings:

    1. Only tempered glass with a width greater than 8 times the thickness is required to drill holes.

    2. For tempered glass with a thickness of no more than 12mm, the interval from the hole edge to the glass margin should not be less than a multiple of the glass thicknessFor tempered glass with a thickness of more than 12mm, the interval from the hole edge to the glass margin should not be less than 2 times the thickness of the glass;

    3. The diameter of the round hole on the tempered glass should be at least larger than the thickness of the glassThe diameter of the round hole should be less than 1 3 of the minimum widthThe radius of the rounding of the corner position of the special-shaped hole in the glass plate should be greater than the thickness of the glass.

  12. Anonymous users2024-01-26

    Chemically tempered glass can be perforated, but it is rare in the market;Physical tempered glass cannot be punched - the whole piece is broken once punched, and this kind of tempered glass is generally available on the market.

  13. Anonymous users2024-01-25

    The finished tempered glass can no longer be punched. This is because during the manufacturing process, the glass is cooled rapidly, and the internal structural stresses should be in a state of equilibrium. If it is punched, it destroys this state and it will break into small grains.

    However, it can be annealed and then tempered. Tempered glass is first punched and then tempered, tempered can not be punched after tempering, tempered glass is processed from ordinary glass, the strength of ordinary glass is greatly improved, and the deformation ability is reduced, so the destruction is all broken.

  14. Anonymous users2024-01-24

    Summary. Tempered glass can also be punched, but if you want to punch holes, you need to meet the corresponding conditions, not all tempered glass can be punched as soon as it comes up, first of all, tempered glass can not be too thin, if it is too thin, it is easy to break when punched.

    Tempered glass can also be punched, but if you want to punch holes, you need to meet the conditions of the corresponding hall, not all the tempered glass can be punched as soon as you come up, first of all, the tempered glass can not be too thin, if it is too thin, it is easy to break when punched. Limb World.

    But I still don't recommend punching.

    The tempered glass that we want to open is 10 mm.

    OK. It's about 40 centimeters.

    Forty centimeters is also OK, provided that the tempered glass can withstand internal and external pressure.

    It should be bearable.

    After all, it's dangerous to not be able to bear it.

    How much does it cost to make such a hole?

    Under normal circumstances, it is 15-30 yuan for an ordinary glass hole to open a hole, which is slightly different in different cities.

    How much is Chengdu City?

    50-70 yuan.

    Is there a professional hole opening master**.

    This is not Sorry.

  15. Anonymous users2024-01-23

    Summary. Hello dear<>

    Glad to answer for you :

    1. How to punch tempered glass.

    1. To punch holes on the tempered glass surface, you first need to prepare an electric drill and a matching drill bit, and you also need to use a special bobbin to punch a round hole. The copper pipe should be prepared first, and at the same time, it should be accurately positioned on the tempered glass, and then the appropriate amount of water should be prepared.

    2. Cover the other parts and punch holes along the top of the mark with an electric drill. With the help of the copper tube to make a round hole, and then rotate the copper tube evenly, it is possible to make an unconventional round hole. When beating, you should also water it at the same time to prevent glass chips from splashing.

    In addition, when punching, it can also be carried out in water, in order to prevent cracks, it must be placed flat during operation, and the force should be even, so that there will be no rupture problem. And it must not hurt anyone, and the staff should take protective measures.

    How to open the hole of tempered glass.

    Hello dear<>

    I'm glad to be able to answer for you: 1. How to punch holes in tempered glass 1. Punch holes on the tempered glass surface, first of all, you need to prepare an electric drill gear and a drill bit to match the sail, and you also need to use a special bobbin to punch a round hole. The copper pipe should be prepared first, and at the same time, it should be accurately positioned on the tempered glass, and then the appropriate amount of water should be prepared.

    2. Cover the other parts and punch holes along the top of the mark with an electric drill. With the help of the copper tube to make a round hole, and then rotate the copper tube evenly, it is possible to make an unconventional round hole. When fighting, the line should also be watered to prevent glass shards from splashing.

    In addition, when punching, it can also be carried out in water, in order to prevent cracks, it must be placed flat during operation, and the force should be even, so that there will be no rupture problem. And it must not hurt anyone, and the staff should take protective measures.

    Can tempered glass open 400x400 holes?

    Hello dear<>

    1. The tempered glass opening can only be carried out if the width of the cover is greater than 8 times the thickness. The thickness of the tempered glass shall not exceed 12 mm in Songbazhou, and the interval from the edge of the hole to the edge of the glass shall not be less than a multiple of the thickness of the glass; If the thickness of the tempered glass balance is more than 12 mm, then the interval from the hole edge to the glass margin should not be less than twice the thickness of the glass.

  16. Anonymous users2024-01-22

    The first thing that can be determined is that tempered glass cannot be punched, and holes can be made before tempering。Tempered glass is ordinary high-grade glass tempered by a high temperature of 800 degrees, the hardness is like steel, it is impossible to punch holes, and all the corners of the four corners are broken with a small tool sled.

    If it has been tempered on the wall, find that the adhesive item is not too heavy, first use adhesive glue on the shelf, and then use glass glue to wipe the shelf all the way, and hang it up when it is dry.

    We often use tempered glass in life, many people don't know how to choose tempered glass, I will tell you about tempered glass.

    Tempered glass, also known as safety glass, is processed more deeply on the basis of ordinary glass, and its advantage is that the hardness is strengthened, and it does not hurt people, and it is more expensive than ordinary glass.

    Punch holes in the tempered glass and the glass will shatter. The production of tempered glass is formed after a certain time and temperature after being processed and made into a pre-set size or shape by ordinary glass, including punching holes and openings. Once the tempered glass is made, there is no way to reprocess it.

    There are two ways to hang items on glass:

    1) Use shadowless glue or good quality structural adhesive to glue the pendant to the required position, and hang the item after the pendant is glued firmly. This kind of glue is called shadowless glue, cured by ultraviolet rays, glued to no trace, according to the distance of the shelf, glued, you can also use good quality glass glue, in short, can not punch, perforated glass will be scrapped, as long as it is not rigid, the way is always more than difficult, in addition to the dead method is a living method.

    2) Change the glass again, make the required holes before tempering, and fix the pendant to the solid wall after the glass replacement is completed, and then install the items.

    The two methods are compared.

    The first kind of saving money and trouble will have the risk of degumming for a certain period of time, and there is a certain risk.

    The second type will be time-consuming and costly, and there will be no hidden dangers in the long run.

    Whichever method you choose, you need to use the most professional people, who have more professional knowledge and tools, and the work will be beautiful.

  17. Anonymous users2024-01-21

    In this regard, I think that tempered glass cannot be opened, because if the tempered glass is opened, it will affect the overall stability of the tempered glass.

  18. Anonymous users2024-01-20

    Tempered glass cannot be opened, because tempered glass is different from ordinary glass, if it is broken, all of it will be broken.

  19. Anonymous users2024-01-19

    I think so. Because many people punch holes in the tempered glass when they decorate.

  20. Anonymous users2024-01-18

    It can't be punched in the tempered glass, it has no toughness, it has to be drilled and then tempered.

  21. Anonymous users2024-01-17

    Punch Method:

    1. Use a glass drill bit: You only need to use a glass drill bit to punch holes in the glass, which is indeed to drill while watering, but it is not necessary to pour too much water. As long as the drill bit does not smoke, take a mineral water bottle, prick a hole in the lid, and use an electric drill to hit it.

    Second, the robust method: remove it, perforate, at present many window glass is tempered glass insulating glass, so first of all, it is necessary to determine the raw material of glass, if it is tempered glass, it can no longer be punched.

    3. If it is ordinary glass, it is also convenient to take it down to find a professional punching machine to punch the hole, plus water cooling, otherwise it will be simply damaged.

  22. Anonymous users2024-01-16

    Wash the glass parts to be processed first, cool dry or tumble dry, and then mark the perforated partsUse a steel file or grinding wheel to burr the perforated or parts that need to be processed, and drip concentrated hydrofluoric acid (.

    Every 1 hour or so, wipe off the residual liquid with a dry cloth and replace it with a new dropAnd so on and so forth. Open.

    It usually takes about 1 day to perforate the glass with a thickness of 1 mm, and it can quickly corrode through the glass plate with a thickness of less than 1 mm, and it takes about 3 days to penetrate the glass plate with a thickness of 2-3 mm.

  23. Anonymous users2024-01-15

    1. Use glass.

    The only way to punch holes in the glass is to use a glass drill bit, which is indeed to drill while watering, but it is not necessary to water too much. As long as the drill bit does not smoke, take a mineral water bottle, pierce two small holes in the lid, and use an electric drill to hit it.

    2. Robust way.

    Remove it and perforate it, at present, many window glass is tempered glass + insulating glass, so first of all, we must determine the glass material, if it is tempered glass, it can no longer be punched;

    3. If it is ordinary glass, it is also best to take it down and find a professional punch machine to punch the hole, plus water cooling, otherwise it is easy to break.

  24. Anonymous users2024-01-14

    At present, it is impossible to punch holes, but 4-7mm steel can be slowly punched and sand can be punched, and 7-15mm steel can be bitten with strong acid.

  25. Anonymous users2024-01-13

    Tempered glass is a compressive stress created on the surface of the glass to counteract the possibility of breakage.

    tensile stress of bad glass, which increases the strength of the glass. Once a devastating trauma is encountered, the whole is broken. Therefore, under normal circumstances, tempered glass can no longer be subjected to this kind of destructive deep processing. The current way of processing is to drill holes before tempering!

Related questions
12 answers2024-02-09

The difference between tempered glass and ordinary glass.

6 answers2024-02-09

You can draw it with a hadron knife, which is sometimes done in my family. But it needs to be a strong person.

16 answers2024-02-09

If you just imitate the sound effect, you can do it from a certain point of view. When playing chords, the 24-hole harmonica is obviously much more powerful than the blues, and the violin blowing of the accented harmonica can barely be simulated if it is monophonic. I've tried the blues 1234 hole pressurization, and the accent harmonica is not too much of a problem.

14 answers2024-02-09

Generally, no, but if you can give enough money, you can transport it by special line. Under normal circumstances, the courier company will not take orders.

23 answers2024-02-09