What should I do if the wood does not dry for two months after the tung paint is applied?

Updated on parenting 2024-08-13
10 answers
  1. Anonymous users2024-02-16

    Reason: Too much humidity in the air and too low temperature.

    Solution: The humidity in the air is too large, the temperature is too low, and the paint dries very slowly. If you have to work in an environment with high humidity, you can add an appropriate amount of slow-drying water to the paint.

    2.Cause: The surface of the furniture contains moisture or grease.

    Solution: Before painting, use a clean soft cloth and wipe around the furniture to remove moisture and keep the surface of the furniture dry. If there is grease on the surface, you can shovel off the paint on the surface, use the heating method to remove the grease, and treat the surface.

    Clean and repaint.

  2. Anonymous users2024-02-15

    The paint is too thick, so that the oxidation is limited to the surface, the solvent at the bottom can not volatilize, the paint film can not be fully dried, different types of paint phase mixing or the use of excessive driers, will make Jiang dry very slowly, resulting in the surface conjunctiva sealing, so that the paint film is slow to dry or even sticky, the construction environment is poor, the paint film is invaded by cold, rain and dew, moisture, etc., or painted in a humid and airless indoor coating, or in the rainy season, foggy construction, the object has a large amount of moisture, In addition, in the cold season, the coating is easy to cause slow drying or improper surface treatment, and there are residual oil, acid, alkali, salt, etc. on the surface of the object, and the pine resin, wax, asphalt that has not been completely removed have not been wiped clean, and the primer has not dried thoroughly to apply the topcoat, etc., which will cause slow or local stickiness, and some even do not dry for a long time.

    To prevent the phenomenon of slow drying of paint, it is necessary to choose high-quality paint for the situation described above, do not mix different types of paint, peel off the object must be treated before painting, remove dirt and moisture, the bottom layer paint is not in the answer to brush the topcoat, when the pine resin that is easy to remove in water should be closed with a sealing primer and then painted, for the long-term adhesive coating must be washed off with gasoline or alkaline water.

  3. Anonymous users2024-02-14

    Summary. The paint is too thick, so that the oxidation is limited to the surface, the solvent at the bottom can not volatilize, the paint film can not be fully dried, different types of paint phase mixing or the use of excessive driers, will make Jiang dry very slowly, resulting in the surface conjunctiva sealing, so that the paint film is slow to dry or even sticky, the construction environment is poor, the paint film is invaded by cold, rain and dew, moisture, etc., or painted in a humid and airless indoor coating, or in the rainy season, foggy construction, the object has a large amount of moisture, In addition, in the cold season, the coating is easy to cause slow drying or improper surface treatment, and there are residual oil, acid, alkali, salt, etc. on the surface of the object, and the pine resin, wax, asphalt that has not been completely removed have not been wiped clean, and the primer has not dried thoroughly to apply the topcoat, etc., which will cause slow or local stickiness, and some even do not dry for a long time.

    To prevent the phenomenon of slow drying of paint, it is necessary to choose high-quality paint for the situation described above, do not mix different types of paint, peel off the object must be treated before painting, remove dirt and moisture, the bottom layer paint is not in the answer to brush the topcoat, when the pine resin that is easy to remove in water should be closed with a sealing primer and then painted, for the long-term adhesive coating must be washed off with gasoline or alkaline water.

    What should I do if the wood does not dry for two months after the tung paint is applied?

    Hello. The paint film layer after one application is too thick, resulting in an increase in drying time and a long-term delay in the paint. Wait a little longer in a ventilated environment for it to become irritated or dry. Or polish off the paint film and re-paint the bridge.

    The paint is too thick, so that the oxidation is limited to the surface, the underlying solvent can not volatilize, the paint film can not be fully dried, different types of paint phase mixing or disturbing Dan with excessive driers, will make Jiang dry very slowly, resulting in the surface conjunctiva sealing, so that the paint film inside the layer of dry slow or even back sticky, poor construction environment, paint film by cold, rain, moisture, etc. invasion or in the humid and air circulation of indoor coating, or in the rainy season, foggy construction, the object has a large amount of moisture, There are residual oil, acid, alkali, salt, etc. on the surface of the object, and the pine resin, wax, and asphalt that have not been completely removed are not wiped clean, and the primer is late and not dry thoroughly, etc., which will cause slow or local stickiness, and some even do not dry for a long time. To prevent the phenomenon of slow drying of paint, it is necessary to choose high-quality paint for the stated situation, do not mix different types of paint, peel off the object before painting must be treated slowly, remove dirt and moisture, the bottom layer is not in the can not be painted with topcoat, when the pine resin that is easy to remove in water should be closed with a sealing primer and then painted, for the long-term adhesive coating must be washed off with gasoline or alkaline water.

  4. Anonymous users2024-02-13

    What should I do if the wood does not dry for two months after the tung paint is applied?

    Hello friends, the paint film layer after one painting is too thick, resulting in an increase in drying time and a long-term delay in the paint. Solution: Wait a little longer for the ventilation ring to dry out on its own. Or polish the paint film off, and re-enter the bend to take the line of paint.

  5. Anonymous users2024-02-12

    What should I do if the wood does not dry for two months after the tung paint is applied?

    The reason why the tung oil brush is not dry on the wood may be due to the wrong time for the slag, it may be that the local temperature has dropped, or the temperature itself is very low, and the tung oil is best to dry faster when it is hot, and it may also be the first line of infiltration and the tung oil is not dry, so that it may be too thick because the brush is too thick to dry out. The most effective and simple way to deal with it is to put the wood in a cool and ventilated place after brushing tung oil, and it will dry naturally in about 2 days. I hope mine is helpful to you and I wish you a happy life <>

  6. Anonymous users2024-02-11

    Summary. Store in a cool, well-ventilated place.

    What should I do if the wood does not dry for two months after the tung paint is applied?

    Store in a cool, well-ventilated place.

    The problem of whether the tung oil brush is dry or not on the wood is closely related to the thickness of the tung oil, the quality of the wood, and the gas of the heavenly sui. If the cooked tung oil brush on the wood does not dry, the effective and simple way to deal with it is to put the wood brushed with tung oil in a cool and ventilated place, and it will dry naturally in about 2 days.

    In addition, if conditions permit, you can borrow the drying room of the paint booth to dry.

    The wood brushed with tung oil is not easy to rot, and its surface will form a protective film, which is not breathable, thus producing a waterproof and anti-corrosion effect.

  7. Anonymous users2024-02-10

    Summers are generally dry for three to seven days, and temperatures below five degrees may be prolonged.

    Based on purity, the raw and cooked performance of tung oil will not affect the drying performance of tung oil, as long as the purity is reached, the raw and cooked drying performance of tung oil is fixed.

    Tung oil is divided into two types: raw tung oil and cooked tung oil, and raw tung oil is used in medicine and chemical industry; Cooked tung oil is processed from raw tung oil, which can replace coatings such as varnish and paint, and is directly used for machine maintenance, indoor wooden floors, wooden ceilings, sauna boards, wooden balcony handrails, etc.; Outdoor wooden flooring, trellises, wooden houses, gazebos, fences, wooden bridges, boats, chairs, wooden farm tools, etc.

    Intuitively, cooked tung oil is thicker than raw tung oil, and the color is dark brown.

    There are two kinds of cooked tung oil, one is cooked pure tung oil, and the other is mixed cooked tung oil.

  8. Anonymous users2024-02-09

    Tung oil is divided into two categories: raw and cooked, and it has to be filtered with gauze before ripening tung oil, so that the effect of rubbing out is better.

    Of course, tung oil is also suitable for other wood, especially outdoor wood, rubbing tung oil is not easy to rot, the surface forms a protective film, not breathable, thus producing waterproof, anti-corrosion effect.

    In addition, tung oil is generally wiped with a clean cotton cloth, not brushed with a brush, the effect of the brush is not good, you have to use a cotton cloth.

    As for how long it will be dry, it depends on the local temperature and humidity, but generally it will dry in about 2 days.

    In addition, it is recommended that you should dry the wood before painting, so as to facilitate the absorption and quick drying of the lacquer.

  9. Anonymous users2024-02-08

    As the saying goes: "air-dried tung oil rain dry paint" depends on your local temperature and humidity and other factors, it is recommended that you wood should be dried before tung oil, which is conducive to the absorption and quick drying of tung oil, good tung oil wood is placed in a ventilated place, generally speaking, the normal weather will be dry for about 3 days.

  10. Anonymous users2024-02-07

    <> "Hello, Kiss! <>

    Tung oil does not dry and can be spraypainted. However, it should be gently sanded, and the varnish effect is better after fine polishing. Generally, it is recommended to brush tung oil first, because the penetration of tung oil is strong, before painting, the surface of the wood should be sanded with sandpaper, which is conducive to penetration, it is recommended to brush twice, and be sure to wait for the first time to completely dry before brushing the second time (Note:

    A kilogram of raw tung oil can be painted with almost 6 10 square meters of wood, but this also depends on the wood and construction conditions) and then you can brush the varnish Note that you must wait for the tung oil to dry naturally before brushing the varnish before brushing the varnish Do not have to polish the wood again Just paint evenly on the surface so that you can achieve mutual protection The protective effect of tung oil on the wood plus the varnish plays a surface role in the wood, and the combination of the two works very well.

Related questions
4 answers2024-08-13

The Regulations on Work-related Injury Insurance stipulate that work-related injuries may be recognized under the following circumstances. >>>More

17 answers2024-08-13

If the business behavior during the period of not applying for a business license is an illegal act of operating without a license, the industrial and commercial department has the right to impose penalties on the behavior, including illegal gains during the period of unlicensed operation and imposing a certain amount of fine. >>>More

24 answers2024-08-13

It's not normal, and after menarche, it usually starts to come regularly every six months, so don't worry. Your condition is perfectly normal.

19 answers2024-08-13

The baby falls off the sofa, immediately to observe whether he falls on the head, and then look at his arms and legs, if the child keeps crying, then it is necessary to go to the hospital for a comprehensive examination, do not delay.

7 answers2024-08-13

First of all, time is the most important thing now.

So don't go page by page now. >>>More